I have collected several sets of worn-out half nuts to rebuild, and was planning to use bearing bronze and silver brazing, but I'm intrigued by the idea of using Delrin or Ertalyte and gluing the threaded liners into the bored-out half nuts. I just did a bit of googling and happened upon the Loctite Design Guide for Bonding Plastic, which is packed with information on different plastics and how well Loctite products work with them. It looks like Loctite 401 is the best choice for either one, and I think I might just give it a try. It will be interesting to find out how good an Acme thread I can cut in Delrin and Ertalyte (and bronze as well, for that matter).
Interestingly, Ertalyte is Polyethylene Terephthalate (PET), commonly known by the trade names Mylar and Dacron.