- Joined
- Jan 20, 2018
- Messages
- 5,922
I find the comments regarding the hardness of dowel pins interesting. Nearly all of the dowels I have worked with were hard, really hard. Like this:
Black-Oxide 1144 Carbon Steel
Not amenable to drilling, tapping or welding. I have seen soft dowels, but mostly in stainless and not very frequently.
Black-Oxide 1144 Carbon Steel
1/4" Dia. | |||||||
---|---|---|---|---|---|---|---|
3/16" Dia. | |||||||
1/8" Dia. | |||||||
Lg. | Dia. Tolerance | Min. Hardness | Breaking Strength, lbs. | Specifications Met | Pkg. Qty. | Pkg. | |
3/8" | 0.0001" to 0.0003" | Rockwell C60 | 2,600 | ASME B18.8.2 | 25 | 98381A302 | $6.60 |
1/2" | 0.0001" to 0.0003" | Rockwell C60 | 2,600 | ASME B18.8.2 | 25 | 98381A304 | 6.73 |
5/8" | 0.0001" to 0.0003" | Rockwell C60 | 2,600 | ASME B18.8.2 | 25 | 98381A306 | 6.90 |
3/4" | 0.0001" to 0.0003" | Rockwell C60 | 2,600 | ASME B18.8.2 | 25 | 98381A308 | 7.05 |
1" | 0.0001" to 0.0003" | Rockwell C60 | 2,600 | ASME B18.8.2 | 25 | 98381A310 | 8.10 |
1/2" | 0.0001" to 0.0003" | Rockwell C60 | 5,900 | ASME B18.8.2 | 25 | 98381A314 | 7.09 |
3/4" | 0.0001" to 0.0003" | Rockwell C60 | 5,900 | ASME B18.8.2 | 25 | 98381A316 | 7.75 |
1" | 0.0001" to 0.0003" | Rockwell C60 | 5,900 | ASME B18.8.2 | 25 | 98381A318 | 8.40 |
1 1/4" | 0.0001" to 0.0003" | Rockwell C60 | 5,900 | ASME B18.8.2 | 25 | 98381A320 | 9.20 |
1 1/2" | 0.0001" to 0.0003" | Rockwell C60 | 5,900 | ASME B18.8.2 | 25 | 98381A322 | 10.32 |
1/2" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A326 | 7.98 |
3/4" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A328 | 8.73 |
1" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A330 | 9.69 |
1 1/4" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A332 | 10.64 |
1 1/2" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A334 | 11.67 |
2" | 0.0001" to 0.0003" | Rockwell C60 | 10,000 | ASME B18.8.2 | 25 | 98381A336 | 1 |
Not amenable to drilling, tapping or welding. I have seen soft dowels, but mostly in stainless and not very frequently.