- Joined
- Oct 11, 2016
- Messages
- 4,008
You might not need to treat the rust pits at all. All you really look for is contact area, and in the number of contact points per inch. Scraping has an averaging effect if done correctly, so missing a spot or 2 won't have much of a difference in the 10-20 rounds of printing/scraping.
If you solder fill, you have to be careful in wipe-downs, that you don't get anything embedded in the soft solder. It can make your day turn bad, and quickly.
I'd clean it up first and print it on a surface plate before doing any refurbishment planning...
If you solder fill, you have to be careful in wipe-downs, that you don't get anything embedded in the soft solder. It can make your day turn bad, and quickly.
I'd clean it up first and print it on a surface plate before doing any refurbishment planning...